:: COMPOSITION ::
|
less
Steel Pipes/Plates
Corbon Steel Pipes/Plates
Alloy Steel Pipes/Plates
Non Ferrous Metal
Pipe Data
Specifications governing Alloy Steel
Tubes are as under:
ASTM A 335 Grade
P - 11 |
ASTM 213 Grade T - 11 |
ASTM A 335 Grade
P - 12 |
ASTM 213
Grade T - 12 |
ASTM A 335 Grade
P - 22 |
ASTM 213 Grade T - 22 |
ASTM A 335 Grade
P - 9 |
ASTM 213 Grade T - 5 |
ASTM A 335 Grade
P - 9 A |
ASTM 213 Grade T - 9 |
ASTM A 335 Grade
P - 5 |
ASTM 213 Grade T - 9 A |
BS 3604 Grade
620 - 440 |
ASTM 213 Grade T - 2 |
BS 3604 Grade
621 |
ASTM 213 Grade T - 1 |
BS 3604 Grade
622 |
ASTM 213 Grade T - 1 B |
BS 3604 Grade
625 |
DIN 17175 15 Mo 3 |
BS 3604 Grade
629 - 470 |
DIN 17175 13 Cr Mo 44 |
BS 3604 Grade
629 - 590 |
DIN 17175 10 Cr Mo 910 |
BS 3604 Grade
660 |
DIN 17175 14 Mo V 63 |
BS 3604 Grade
762 |
DIN 17175 X 20 Cr Mo V 121 |
|
BS 3059 Grade 243 |
BS
3059 Grade 620 - 460 |
BS 3059 Grade
622 - 490 |
BS
3059 Grade 629 - 470 |
BS 3059 Grade
629 - 590 |
BS
3059 Grade 762 |
IS 2002-62 STEEL PLATED FOR BOILERS
|
Chemical Composition,%
|
Tensile Test
|
Designation |
C max. |
Si |
P max |
S max |
Tensile Strength Kgf/mm2 |
Yield Point Kgf/mm2,min. |
Elongation |
Test
Piece |
%, min |
IS 2002-1 |
0.18 |
.010-0.35 |
0.40 |
0.40 |
37-45 |
55 |
5.65/So
4/So |
26
30 |
IS 2002-2A |
0.20 |
0.10-0.35 |
0.050 |
0.050 |
42-50 |
50 |
5.65/So
4/So |
25
29 |
IS 2002-2b |
0.22 |
0.10-0.35 |
0.050 |
0.050 |
52-62 |
50 |
5.65/So
4/So |
20
24 |
Kawasaki Specification [AG] Steel Plates for
Galvanizing Pots
|
Chemical
Composition,% |
Tensile Test
|
Bend test
|
Designation |
C
Si Mn P S
Max Max
Max |
Yield
Point Tensile Strength
Kgf/mm2 Kgf/mm2.(N/mm2) |
Elongation
%, Test Piece |
Angle of Bend |
Inside
Radius |
AG |
0.09 tr.0.20-0.40 0.30
0.030 |
--
-- |
--
-- |
|
|
ASTM A 285-78 Pressure Vessel Plates, Carbon
Steel, Low - and Intermediate- Tensile Strength
|
Chemical Composition,% |
Tensile
Test*1
|
1.
(i) Refer to (1) for ASTM A 203
(ii) Refer to (2) for ASTM A 203
(iii) Refer to (4) for ASTM A 203. |
Designation |
C max |
Mn max |
P max |
S max |
Tensile Strength
ksi (MPa), |
Yeild Strengh ksi(MPa),min. |
Elongation,% min |
GL=8 in.
GL=2 in
|
A 285 A |
0.17 |
0.90 |
0.035 |
0.040 |
45-65 (310-450) |
24(165) |
27
30
|
A 285 B |
0.22 |
0.90 |
0.035 |
0.040 |
50-70(385-485) |
27(185) |
25
28 |
A 285 C |
0.28 |
0.90 |
0.035 |
0.040 |
55-75(380-515) |
30(205) |
23
27 |
|
|
Contact
Us: 132, Kika Street, Gulalwadi, Mumbai- 400 004 (INDIA), Phone No : 91
- 22- 5639 4091, 2242 1422, 2242 3277, Fax : 91 - 22 - 2242 4558
Design & Developed By:
Mesotek
|